China Mechanical Engineering ›› 2013, Vol. 24 ›› Issue (02): 158-162.

Previous Articles     Next Articles

Effects of  Packing Time on Relative Refractive Index of Microinjection Molded Plano-lenses

Yang Can;Yin Xiaohong   

  1. Zhejiang Normal University,Jinhua,Zhejiang,321004
  • Online:2013-01-25 Published:2013-02-01
  • Supported by:
     
    Zhejiang Provincial Scientific Research Project of Ministry of Education of China(No. Y201225768)

微注塑保压时间对平面透镜相对折射率的影响

杨灿;尹晓红   

  1. 浙江师范大学,金华,321004
  • 基金资助:
    浙江省“钱江人才计划”特殊急需类资助项目(QJD1202005);浙江省教育厅科研项目(Y201225768);浙江师范大学重大科技专项预研项目(KJ20120013) 
    Zhejiang Provincial Scientific Research Project of Ministry of Education of China(No. Y201225768)

Abstract:

Based on the facts that transparent devices required excellent optical properties,an approach  was proposed for controlling devices' optical properties by investigating and controlling the relative refractive index.Taking the microinjection molded thin optical lens as an example,the wavefront of a parallel laser light source coming through the optical devices was measured and reconstructed.Then the theoretical relationship between the reconstructed wavefront and the relative refractive index was analyzed
and deduced,and the relative refractive index distributions of the optical
lenses were calculated.At last,the packing time's effects in microinjection molding on the relative refractive index distribution were  investigated.
The experimental results show that as the packing time increases from 1s to 3s,the relative refractive index distribution inside the lenses is more uniform,and the range of the refractive index decreases from
6.1×10-3 to 2.9×10-3.The proposed characterization method with respect to relative refractive index is effective for controlling the optical devices' properties. 

Key words: microinjection molding, packing time, wavefront reconstruction, relative refractive index

摘要:

针对透明器件对光学性能要求很高的现实,提出通过调控相对折射率来实现光学性能调控的方法。以微注塑薄壁透镜为例,对平行激光光源通过光学透镜后的波阵面进行检测与重建;接着推导出了波阵面检测结果与相对折射率的理论关系,并计算了透镜内部相对折射率的分布;最后考查了微注塑过程中保压时间对透镜相对折射率分布的影响。实验结果表明:当微注塑保压时间从1s延长至3s时,相对折射率分布均匀度明显提高,折射率的极差从6.1×10-3减小到2.9×10-3。该相对折射率表征方法能有效调控光学制品性能。

关键词: 微注塑, 保压时间, 波阵面重建, 相对折射率

CLC Number: